Additions to be made to compensate for HangUp and Degassing & Mellting Pots

There is always resin left behind in a degassing vessel or melting pot.  Keep records so that you are aware of what happens in your plant.

If 3 Kg 10T90 is expected to be left behind in the degassing vessel, and 0.4 Kg MOCA in the melting pot, these figures should be added to the quantity melted or degassed if no more castings are expected.  It is equally important to have enough material ready to cast.

Example:

10T90:   200.82 +  3    =  203.82   Kg 10T90 minimum
MOCA
:   25.18   + 0.4  =  25.58     Kg MOCA minimum




Copyright © 2010, all rights reserved. Disclaimer